China Influence of Laser Cladding Process Parameters on Forming Quality - China Supplier China Influence of Laser Cladding Process Parameters on Forming Quality - China Supplier China Influence of Laser Cladding Process Parameters on Forming Quality - China Supplier China Influence of Laser Cladding Process Parameters on Forming Quality - China Supplier

Influence of Laser Cladding Process Parameters on Forming Quality

Price:Negotiable
Industry Category:
Product Category:
Brand: 國盛激光
Spec:


Contact Info
  • Add:西安市國家民用航天產(chǎn)業(yè)基地航天基地299號西安建工科技創(chuàng)業(yè)基地十號樓4層, Zip:
  • Contact: 段純
  • Tel:17392761868
  • Email:gsjgkj@163.com

Other Products

Description
Additional Information

Influence of Process Parameters on Forming Quality

1. Laser Power: The power directly affects the amount of powder that can be melted per unit time, influencing the cladding efficiency. When other working parameters are fixed, insufficient power may result in incomplete powder melting, pitting after polishing, inadequate bonding strength, and low coating hardness. Excessive power may cause overmelting of the melt track, leading to the appearance of oblique wrinkles on the surface.

2. Powder Feed Rate: After the powder stream interacts with the laser, it absorbs laser energy. A higher powder feed rate results in more absorbed laser energy. If the powder feed rate is too high, it may lead to insufficient laser energy, resulting in an unmelted coating, pitting after polishing, and failure to melt the substrate, preventing metallurgical bonding between the coating and substrate and causing coating peeling. A high powder feed rate leads to low powder utilization, while a low powder feed rate results in high powder utilization.

3. Scanning Speed: A higher scanning speed results in a thinner cladding layer, while a lower scanning speed results in a thicker cladding layer. Excessive scanning speed may prevent the formation of a molten pool on the substrate, leading to poor metallurgical bonding between the coating and substrate, slow cooling of the melt track, an excessively long red tail, and peeling. A lower scanning speed can improve coating hardness and powder utilization.

4. Step Over: A smaller step over results in a higher overlap rate and a smoother coating surface, while a larger step over results in a lower overlap rate and more pronounced coating streaks. The step over affects the dilution rate. A smaller step over results in less laser energy reaching the substrate, leading to a lower dilution rate. A larger step over results in more laser energy reaching the substrate, leading to a higher dilution rate.

5. Gas Flow Rate: The gas serves two purposes: transporting the powder and protecting the high-temperature coating from oxidation. Insufficient gas flow may cause powder clogging, while excessive gas flow may result in high powder velocity, significant bouncing, and low powder utilization. Generally, argon provides better protection for the coating than nitrogen, resulting in higher coating quality.

6. Nozzle Height: If the nozzle is too high, the powder dispersion increases, leading to low powder utilization. If it is too low, the nozzle is prone to powder adhesion during the cladding process.

Industry Category
Product Category
Brand: 國盛激光
Spec:
Stock:
Origin: China / Shaanxi / Xianshi
About Toocle.com - Partner Programme - Old Version
Copyright ? Toocle.com. All Rights Reserved.
(浙)-經(jīng)營性-2023-0192
ChatGlobal Chat Now 白银市| 抚顺县| 镇坪县| 汝阳县| 阿尔山市| 新余市| 达日县| 革吉县| 永昌县| 西昌市| 禹州市| 双辽市| 高邮市| 定日县| 大埔区| 成武县| 兰西县| 措美县| 昌邑市| 苏尼特右旗| 神农架林区| 岳池县| 社会| 临桂县| 芦溪县| 内丘县| 山阴县| 新泰市| 柏乡县| 木里| 乌拉特前旗| 荆门市| 全椒县| 西峡县| 砀山县| 二连浩特市| 方山县| 五常市| 高阳县| 高唐县| SHOW|